Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 8.57 g/cm³ Show Material materials with Dichte of 8.57 g/cm³ | Typical for Niobium |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 104 GPa Show Material materials with Elastizitätsmodul of 104 GPa | Typical for Niobium |
Elongation A25 | 20.0 °C | 20 % Show Material materials with Elongation A25 of 20 % | |
1100.0 °C | 20 % Show Material materials with Elongation A25 of 20 % | ||
Poissonzahl | 23.0 °C | 0.4 [-] Show Material materials with Poissonzahl of 0.4 [-] | Typical for Niobium |
Schubmodule | 23.0 °C | 38 GPa Show Material materials with Schubmodule of 38 GPa | Typical for Niobium |
Streckgrenze Rp 0,2 | 20.0 °C | 260 - 275 MPa Show Material materials with Streckgrenze Rp 0,2 of 260 - 275 MPa | |
1100.0 °C | 110 MPa Show Material materials with Streckgrenze Rp 0,2 of 110 MPa | ||
Zugfestigkeit | 20.0 °C | 370 - 385 MPa Show Material materials with Zugfestigkeit of 370 - 385 MPa | |
1100.0 °C | 145 MPa Show Material materials with Zugfestigkeit of 145 MPa | ||
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 6.8E-6 - 1.4E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 6.8E-6 - 1.4E-5 1/K | Typical for Niobium |
Schmelzpunkt | 2468 °C Show Material materials with Schmelzpunkt of 2468 °C | Typical for Niobium | |
Spezifische Wärmekapazität | 23.0 °C | 201 - 272 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 201 - 272 J/(kg·K) | Typical for Niobium |
Wärmeleitfähigkeit | 23.0 °C | 53 - 54 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 53 - 54 W/(m·K) | Typical for Niobium |
Chemical properties
Property | Value |
---|---|
Hafnium | 9 - 11 % Show Material materials with Hafnium of 9 - 11 % |
Kohlenstoff | 0.015 % Show Material materials with Kohlenstoff of 0.015 % |
Sauerstoff | 0.03 % Show Material materials with Sauerstoff of 0.03 % |
Stickstoff | 0.01 % Show Material materials with Stickstoff of 0.01 % |
Tantal | 0.5 % Show Material materials with Tantal of 0.5 % |
Titan | 0.7 - 1.3 % Show Material materials with Titan of 0.7 - 1.3 % |
Wasserstoff | 1.5E-3 % Show Material materials with Wasserstoff of 1.5E-3 % |
Wolfram | 0.5 % Show Material materials with Wolfram of 0.5 % |
Zirkonium | 0.7 % Show Material materials with Zirkonium of 0.7 % |