Mechanisch
Property | Temperature | Value |
---|---|---|
Elastizitätsmodul | 20.0 °C | 190 GPa Show Material materials with Elastizitätsmodul of 190 GPa |
100.0 °C | 187 GPa Show Material materials with Elastizitätsmodul of 187 GPa | |
150.0 °C | 185 GPa Show Material materials with Elastizitätsmodul of 185 GPa | |
200.0 °C | 183 GPa Show Material materials with Elastizitätsmodul of 183 GPa | |
230.0 °C | 182 GPa Show Material materials with Elastizitätsmodul of 182 GPa | |
Härte, Vickers | 20.0 °C | 150 [-] Show Material materials with Härte, Vickers of 150 [-] |
Chemical properties
Property | Value |
---|---|
Eisen | 0.01 % Show Material materials with Eisen of 0.01 % |
Kohlenstoff | 3E-3 - 5E-3 % Show Material materials with Kohlenstoff of 3E-3 - 5E-3 % |
Molybdän | 0.01 - 0.02 % Show Material materials with Molybdän of 0.01 - 0.02 % |
Nickel | 5E-3 % Show Material materials with Nickel of 5E-3 % |
Niobium | 0.04 - 0.1 % Show Material materials with Niobium of 0.04 - 0.1 % |
Silizium | 2.5E-3 - 5E-3 % Show Material materials with Silizium of 2.5E-3 - 5E-3 % |
Stickstoff | 3E-3 - 5E-3 % Show Material materials with Stickstoff of 3E-3 - 5E-3 % |
Titan | 4E-3 - 5E-3 % Show Material materials with Titan of 4E-3 - 5E-3 % |
Wasserstoff | 5E-4 - 1E-3 % Show Material materials with Wasserstoff of 5E-4 - 1E-3 % |
Wolfram | 2.2 - 3.5 % Show Material materials with Wolfram of 2.2 - 3.5 % |