Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 9.6 g/cm³ Show Material materials with Dichte of 9.6 g/cm³ | Typical for Lead Antimony |
Mechanisch
Property | Temperature | Value |
---|---|---|
Härte, Brinell | 20.0 °C | 18 [-] Show Material materials with Härte, Brinell of 18 [-] |
50.0 °C | 15 [-] Show Material materials with Härte, Brinell of 15 [-] | |
120.0 °C | 14 [-] Show Material materials with Härte, Brinell of 14 [-] | |
150.0 °C | 10 [-] Show Material materials with Härte, Brinell of 10 [-] | |
Streckgrenze Rp 0,2 | 20.0 °C | 39 MPa Show Material materials with Streckgrenze Rp 0,2 of 39 MPa |
50.0 °C | 37 MPa Show Material materials with Streckgrenze Rp 0,2 of 37 MPa | |
100.0 °C | 25 MPa Show Material materials with Streckgrenze Rp 0,2 of 25 MPa | |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzpunkt | 235 - 305 °C Show Material materials with Schmelzpunkt of 235 - 305 °C | Typical for Lead Antimony | |
Spezifische Wärmekapazität | 23.0 °C | 130 - 159 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 130 - 159 J/(kg·K) | Typical for Lead Antimony |
Wärmeleitfähigkeit | 23.0 °C | 24 - 34 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 24 - 34 W/(m·K) | Typical for Lead Antimony |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 % Show Material materials with Aluminium of 0.01 % |
Antimon | 13.5 - 15.5 % Show Material materials with Antimon of 13.5 - 15.5 % |
Arsen | 0.8 - 1.2 % Show Material materials with Arsen of 0.8 - 1.2 % |
Bismut | 0.1 % Show Material materials with Bismut of 0.1 % |
Eisen | 0.1 % Show Material materials with Eisen of 0.1 % |
Kupfer | 0.7 % Show Material materials with Kupfer of 0.7 % |
Zink | 0.01 % Show Material materials with Zink of 0.01 % |
Zinn | 0.9 - 1.7 % Show Material materials with Zinn of 0.9 - 1.7 % |