Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 10.3 g/cm³ Show Material materials with Dichte of 10.3 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Streckgrenze Rp 0,2 | 20.0 °C | 27 - 39 MPa Show Material materials with Streckgrenze Rp 0,2 of 27 - 39 MPa |
Thermisch
Property | Value |
---|---|
Schmelzpunkt | 260 °C Show Material materials with Schmelzpunkt of 260 °C |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 % Show Material materials with Aluminium of 0.01 % |
Antimon | 9 - 11 % Show Material materials with Antimon of 9 - 11 % |
Arsen | 0.25 % Show Material materials with Arsen of 0.25 % |
Bismut | 0.1 % Show Material materials with Bismut of 0.1 % |
Eisen | 0.1 % Show Material materials with Eisen of 0.1 % |
Kupfer | 0.7 % Show Material materials with Kupfer of 0.7 % |
Zink | 0.01 % Show Material materials with Zink of 0.01 % |
Zinn | 5 - 7 % Show Material materials with Zinn of 5 - 7 % |