Mechanisch
Property | Temperature | Value |
---|---|---|
Härte, Brinell | 20.0 °C | 25 [-] Show Material materials with Härte, Brinell of 25 [-] |
50.0 °C | 20 [-] Show Material materials with Härte, Brinell of 20 [-] | |
120.0 °C | 12 [-] Show Material materials with Härte, Brinell of 12 [-] | |
150.0 °C | 8 [-] Show Material materials with Härte, Brinell of 8 [-] | |
Streckgrenze Rp 0,2 | 20.0 °C | 61 MPa Show Material materials with Streckgrenze Rp 0,2 of 61 MPa |
50.0 °C | 60 MPa Show Material materials with Streckgrenze Rp 0,2 of 60 MPa | |
100.0 °C | 36 MPa Show Material materials with Streckgrenze Rp 0,2 of 36 MPa | |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzpunkt | 215 - 350 °C Show Material materials with Schmelzpunkt of 215 - 350 °C | Typical for Tin Antimony | |
Wärmeleitfähigkeit | 23.0 °C | 40 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 40 W/(m·K) | Typical for Tin Antimony |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 % Show Material materials with Aluminium of 0.01 % |
Antimon | 11 - 13 % Show Material materials with Antimon of 11 - 13 % |
Arsen | 0.1 % Show Material materials with Arsen of 0.1 % |
Bismut | 0.08 % Show Material materials with Bismut of 0.08 % |
Blei | 1 - 3 % Show Material materials with Blei of 1 - 3 % |
Eisen | 0.1 % Show Material materials with Eisen of 0.1 % |
Kupfer | 5 - 7 % Show Material materials with Kupfer of 5 - 7 % |
Zink | 0.01 % Show Material materials with Zink of 0.01 % |