Mechanisch
Property | Temperature | Value |
---|---|---|
Härte, Brinell | 20.0 °C | 22 [-] Show Material materials with Härte, Brinell of 22 [-] |
50.0 °C | 17 [-] Show Material materials with Härte, Brinell of 17 [-] | |
100.0 °C | 10 [-] Show Material materials with Härte, Brinell of 10 [-] | |
120.0 °C | 11 [-] Show Material materials with Härte, Brinell of 11 [-] | |
150.0 °C | 8 [-] Show Material materials with Härte, Brinell of 8 [-] | |
Streckgrenze Rp 0,2 | 20.0 °C | 46 - 47 MPa Show Material materials with Streckgrenze Rp 0,2 of 46 - 47 MPa |
50.0 °C | 44 MPa Show Material materials with Streckgrenze Rp 0,2 of 44 MPa | |
100.0 °C | 27 MPa Show Material materials with Streckgrenze Rp 0,2 of 27 MPa | |
Zugfestigkeit | 20.0 °C | 77 MPa Show Material materials with Zugfestigkeit of 77 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzpunkt | 215 - 350 °C Show Material materials with Schmelzpunkt of 215 - 350 °C | Typical for Tin Antimony | |
Wärmeleitfähigkeit | 23.0 °C | 40 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 40 W/(m·K) | Typical for Tin Antimony |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.01 % Show Material materials with Aluminium of 0.01 % |
Antimon | 7 - 8 % Show Material materials with Antimon of 7 - 8 % |
Arsen | 0.1 % Show Material materials with Arsen of 0.1 % |
Bismut | 0.08 % Show Material materials with Bismut of 0.08 % |
Blei | 0.35 % Show Material materials with Blei of 0.35 % |
Cadmium | 0.05 % Show Material materials with Cadmium of 0.05 % |
Eisen | 0.1 % Show Material materials with Eisen of 0.1 % |
Kupfer | 3 - 4 % Show Material materials with Kupfer of 3 - 4 % |
Zink | 0.01 % Show Material materials with Zink of 0.01 % |