Allgemein
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Dichte | 2.84 g/cm³ Show Material materials with Dichte of 2.84 g/cm³ | T6 | WL 3.1754 | Casting | |
20.0 °C | 2.84 g/cm³ Show Material materials with Dichte of 2.84 g/cm³ | T6 | WL 3.1854, WL 3.1754 |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Dehnung | 1.0 % Show Material materials with Dehnung of 1.0 % | T6 | WL 3.1754 | Casting | A50 | |
20.0 °C | 1.0 % Show Material materials with Dehnung of 1.0 % | T6 | WL 3.1854, WL 3.1754 | |||
Elastizitätsmodul | 70.0 GPa Show Material materials with Elastizitätsmodul of 70.0 GPa | T6 | WL 3.1754 | Casting | ||
20.0 °C | 70.0 GPa Show Material materials with Elastizitätsmodul of 70.0 GPa | T6 | WL 3.1854, WL 3.1754 | |||
Härte, Brinell | 80.0 [-] Show Material materials with Härte, Brinell of 80.0 [-] | T6 | WL 3.1754 | Casting | ||
20.0 °C | 80.0 [-] Show Material materials with Härte, Brinell of 80.0 [-] | T6 | WL 3.1854, WL 3.1754 | |||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Cast 2xx.x Series Aluminium | ||||
Zugfestigkeit | 180.0 MPa Show Material materials with Zugfestigkeit of 180.0 MPa | T6 | WL 3.1754 | Casting | ||
190.0 MPa Show Material materials with Zugfestigkeit of 190.0 MPa | T6 | WL 3.1754 | Casting | |||
20.0 °C | 180.0 MPa Show Material materials with Zugfestigkeit of 180.0 MPa | T6 | WL 3.1854, WL 3.1754 | |||
20.0 °C | 185.0 MPa Show Material materials with Zugfestigkeit of 185.0 MPa | T6 | WL 3.1854, WL 3.1754 | |||
20.0 °C | 190.0 MPa Show Material materials with Zugfestigkeit of 190.0 MPa | T6 | WL 3.1854, WL 3.1754 | |||
20.0 °C | 200.0 MPa Show Material materials with Zugfestigkeit of 200.0 MPa | T6 | WL 3.1854, WL 3.1754 | |||
20.0 °C | 215.0 MPa Show Material materials with Zugfestigkeit of 215.0 MPa | T6 | WL 3.1854, WL 3.1754 |
Thermisch
Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 20 °C | 1.9999999999999998e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.9999999999999998e-05 1/K | T6 | WL 3.1754 | Casting | |
100 °C | 1.9999999999999998e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.9999999999999998e-05 1/K | T6 | WL 3.1754 | Casting | ||
Schmelzpunkt | 510.0 - 790.0 °C Show Material materials with Schmelzpunkt of 510.0 - 790.0 °C | Typical for Cast 2xx.x Series Aluminium | ||||
Spezifische Wärmekapazität | 875.0 - 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 875.0 - 963.0 J/(kg·K) | Typical for Cast 2xx.x Series Aluminium | ||||
Wärmeleitfähigkeit | 155 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 155 W/(m·K) | T6 | WL 3.1754 | Casting | ||
20.0 °C | 155.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 155.0 W/(m·K) | T6 | WL 3.1854, WL 3.1754 |
Elektrisch
Property | Temperature | Value | Condition | Related Standards | Shape |
---|---|---|---|---|---|
Elektrische Leitfähigkeit | 21000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 21000000.0 S/m | T6 | WL 3.1754 | Casting | |
20.0 °C | 21000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 21000000.0 S/m | T6 | WL 3.1854, WL 3.1754 | ||
spezifischer Widerstand | 4.76e-08 Ω·m Show Material materials with spezifischer Widerstand of 4.76e-08 Ω·m | T6 | WL 3.1754 | Casting |
Chemical properties
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Aluminium | 93.4 % Show Material materials with Aluminium of 93.4 % | T6 | WL 3.1854, WL 3.1754 | |
Eisen | 0.35 % Show Material materials with Eisen of 0.35 % | T6 | WL 3.1854, WL 3.1754 | |
0.50 % Show Material materials with Eisen of 0.50 % | T6 | WL 3.1754 | Casting | |
Kupfer | 4.2 - 5.0 % Show Material materials with Kupfer of 4.2 - 5.0 % | T6 | WL 3.1854, WL 3.1754 | |
4.5 - 5.5 % Show Material materials with Kupfer of 4.5 - 5.5 % | T6 | WL 3.1754 | Casting | |
Magnesium | 0.15 - 0.35 % Show Material materials with Magnesium of 0.15 - 0.35 % | T6 | WL 3.1854, WL 3.1754 | |
Mangan | 0.1 % Show Material materials with Mangan of 0.1 % | T6 | WL 3.1854, WL 3.1754 | |
0.2 - 0.3 % Show Material materials with Mangan of 0.2 - 0.3 % | T6 | WL 3.1754 | Casting | |
Nickel | 0.03 % Show Material materials with Nickel of 0.03 % | T6 | WL 3.1854, WL 3.1754 | |
1.3 - 1.8 % Show Material materials with Nickel of 1.3 - 1.8 % | T6 | WL 3.1754 | Casting | |
Silizium | 0.3 % Show Material materials with Silizium of 0.3 % | T6 | WL 3.1854, WL 3.1754 | Casting |
Titan | 0.15 - 0.25 % Show Material materials with Titan of 0.15 - 0.25 % | T6 | WL 3.1854, WL 3.1754 | Casting |
Zink | 0.1 Show Material materials with Zink of 0.1 | T6 | WL 3.1854, WL 3.1754 | |
Zirkonium | 0.1 - 0.3 % Show Material materials with Zirkonium of 0.1 - 0.3 % | T6 | WL 3.1754 | Casting |
Technological properties
Property | ||
---|---|---|
Processing methods | investment casting, sample taken from casting |