Allgemein
Property | Temperature | Value | Condition | Related Standards |
---|---|---|---|---|
Dichte | 20.0 °C | 2.7 g/cm³ Show Material materials with Dichte of 2.7 g/cm³ | H3x | WL 3.2134 |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Dehnung | 20.0 °C | 0.5 % Show Material materials with Dehnung of 0.5 % | H3x | WL 3.2134 | |
20.0 °C | 1.0 % Show Material materials with Dehnung of 1.0 % | H3x | WL 3.2134 | ||
20.0 °C | 1.5 % Show Material materials with Dehnung of 1.5 % | H3x | WL 3.2134 | ||
20.0 °C | 2.0 % Show Material materials with Dehnung of 2.0 % | H3x | WL 3.2134 | ||
Elastizitätsmodul | 20.0 °C | 71.0 GPa Show Material materials with Elastizitätsmodul of 71.0 GPa | H3x | WL 3.2134 | |
Härte, Brinell | 20.0 °C | 60.0 [-] Show Material materials with Härte, Brinell of 60.0 [-] | H3x | WL 3.2134 | |
20.0 °C | 65.0 [-] Show Material materials with Härte, Brinell of 65.0 [-] | H3x | WL 3.2134 | ||
20.0 °C | 70.0 [-] Show Material materials with Härte, Brinell of 70.0 [-] | H3x | WL 3.2134 | ||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Cast 3xx.x Series Aluminium | |||
Scherfestigkeit | 20.0 °C | 120.0 MPa Show Material materials with Scherfestigkeit of 120.0 MPa | H3x | WL 3.2134 | |
20.0 °C | 160.0 MPa Show Material materials with Scherfestigkeit of 160.0 MPa | H3x | WL 3.2134 | ||
Schubmodule | 2.8 GPa Show Material materials with Schubmodule of 2.8 GPa | Typical for Cast 3xx.x Series Aluminium | |||
Zugfestigkeit | 20.0 °C | 150.0 MPa Show Material materials with Zugfestigkeit of 150.0 MPa | H3x | WL 3.2134 | |
20.0 °C | 160.0 MPa Show Material materials with Zugfestigkeit of 160.0 MPa | H3x | WL 3.2134 | ||
20.0 °C | 180.0 MPa Show Material materials with Zugfestigkeit of 180.0 MPa | H3x | WL 3.2134 | ||
20.0 °C | 190.0 MPa Show Material materials with Zugfestigkeit of 190.0 MPa | H3x | WL 3.2134 |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.6e-05 - 2.3e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6e-05 - 2.3e-05 1/K | Typical for Cast 3xx.x Series Aluminium |
Schmelzpunkt | 505.0 - 770.0 °C Show Material materials with Schmelzpunkt of 505.0 - 770.0 °C | Typical for Cast 3xx.x Series Aluminium |
Spezifische Wärmekapazität | 960.0 - 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 960.0 - 963.0 J/(kg·K) | Typical for Cast 3xx.x Series Aluminium |
Wärmeleitfähigkeit | 130.0 - 180.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 130.0 - 180.0 W/(m·K) | Typical for Cast 3xx.x Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Chrom | 0.25 Show Material materials with Chrom of 0.25 | H3x | WL 3.2134 |
Eisen | 0.6 Show Material materials with Eisen of 0.6 | H3x | WL 3.2134 |
Kupfer | 1.0 - 1.5 % Show Material materials with Kupfer of 1.0 - 1.5 % | H3x | WL 3.2134 |
Magnesium | 0.4 - 0.6 % Show Material materials with Magnesium of 0.4 - 0.6 % | H3x | WL 3.2134 |
Mangan | 0.5 Show Material materials with Mangan of 0.5 | H3x | WL 3.2134 |
Silizium | 4.5 - 5.5 % Show Material materials with Silizium of 4.5 - 5.5 % | H3x | WL 3.2134 |
Titan | 0.25 Show Material materials with Titan of 0.25 | H3x | WL 3.2134 |
Zink | 0.3 Show Material materials with Zink of 0.3 | H3x | WL 3.2134 |
Technological properties
Property | ||
---|---|---|
Processing methods | permanent mould casting |