Allgemein
Property | Temperature | Value | Condition | Related Standards |
---|---|---|---|---|
Dichte | 20.0 °C | 2.7 g/cm³ Show Material materials with Dichte of 2.7 g/cm³ | H3x | WL 3.2364 |
Mechanisch
Property | Temperature | Value | Condition | Related Standards | Comment |
---|---|---|---|---|---|
Dehnung | 20.0 °C | 2.0 % Show Material materials with Dehnung of 2.0 % | H3x | WL 3.2364 | |
Elastizitätsmodul | 20.0 °C | 70.6 GPa Show Material materials with Elastizitätsmodul of 70.6 GPa | H3x | WL 3.2364 | |
Härte, Brinell | 20.0 °C | 60.0 [-] Show Material materials with Härte, Brinell of 60.0 [-] | H3x | WL 3.2364 | |
20.0 °C | 65.0 [-] Show Material materials with Härte, Brinell of 65.0 [-] | H3x | WL 3.2364 | ||
20.0 °C | 70.0 [-] Show Material materials with Härte, Brinell of 70.0 [-] | H3x | WL 3.2364 | ||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Cast 3xx.x Series Aluminium | |||
Scherfestigkeit | 20.0 °C | 137.0 MPa Show Material materials with Scherfestigkeit of 137.0 MPa | H3x | WL 3.2364 | |
Schubmodule | 2.8 GPa Show Material materials with Schubmodule of 2.8 GPa | Typical for Cast 3xx.x Series Aluminium | |||
Zugfestigkeit | 20.0 °C | 118.0 MPa Show Material materials with Zugfestigkeit of 118.0 MPa | H3x | WL 3.2364 | |
20.0 °C | 137.0 MPa Show Material materials with Zugfestigkeit of 137.0 MPa | H3x | WL 3.2364 | ||
20.0 °C | 157.0 MPa Show Material materials with Zugfestigkeit of 157.0 MPa | H3x | WL 3.2364 | ||
20.0 °C | 186.0 MPa Show Material materials with Zugfestigkeit of 186.0 MPa | H3x | WL 3.2364 |
Thermisch
Property | Value | Comment |
---|---|---|
Koeffizient der thermischen Ausdehnung | 1.6e-05 - 2.3e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6e-05 - 2.3e-05 1/K | Typical for Cast 3xx.x Series Aluminium |
Schmelzpunkt | 505.0 - 770.0 °C Show Material materials with Schmelzpunkt of 505.0 - 770.0 °C | Typical for Cast 3xx.x Series Aluminium |
Spezifische Wärmekapazität | 960.0 - 963.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 960.0 - 963.0 J/(kg·K) | Typical for Cast 3xx.x Series Aluminium |
Wärmeleitfähigkeit | 130.0 - 180.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 130.0 - 180.0 W/(m·K) | Typical for Cast 3xx.x Series Aluminium |
Chemical properties
Property | Value | Condition | Related Standards |
---|---|---|---|
Eisen | 0.6 Show Material materials with Eisen of 0.6 | H3x | WL 3.2364 |
Kupfer | 0.2 Show Material materials with Kupfer of 0.2 | H3x | WL 3.2364 |
Magnesium | 0.2 - 0.4 % Show Material materials with Magnesium of 0.2 - 0.4 % | H3x | WL 3.2364 |
Mangan | 0.35 Show Material materials with Mangan of 0.35 | H3x | WL 3.2364 |
Silizium | 6.5 - 7.5 % Show Material materials with Silizium of 6.5 - 7.5 % | H3x | WL 3.2364 |
Titan | 0.25 Show Material materials with Titan of 0.25 | H3x | WL 3.2364 |
Zink | 0.3 Show Material materials with Zink of 0.3 | H3x | WL 3.2364 |
Technological properties
Property | ||
---|---|---|
Processing methods | permanent mould casting, sample taken from casting |