Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 10.7 g/cm³ Show Material materials with Dichte of 10.7 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Härte, Brinell | 20.0 °C | 12 [-] Show Material materials with Härte, Brinell of 12 [-] |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzpunkt | 235 - 305 °C Show Material materials with Schmelzpunkt of 235 - 305 °C | Typical for Lead Antimony | |
Spezifische Wärmekapazität | 23.0 °C | 130 - 159 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 130 - 159 J/(kg·K) | Typical for Lead Antimony |
Wärmeleitfähigkeit | 23.0 °C | 24 - 34 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 24 - 34 W/(m·K) | Typical for Lead Antimony |
Chemical properties
Property | Value |
---|---|
Antimon | 7 - 9 % Show Material materials with Antimon of 7 - 9 % |