Wrought Copper Bronze Aluminium Bronze
AMPCO® 21 Extruded and drawn rounds and rectangular barsSuministrada por:
AMPCO METALWrought Copper Bronze Aluminium Bronze
EN 12163 Grade CuAl11Fe6Ni6 R830Wrought Copper Bronze Aluminium Bronze
EN 12165 Grade CuAl11Fe6Ni6 H190Wrought Copper Bronze Aluminium Bronze
EN 12163 Grade CuAl11Fe6Ni6 R750Wrought Copper Bronze Aluminium Bronze
EN 12163 Grade CuAl11Fe6Ni6 H230Wrought Copper Bronze Aluminium Bronze
EN 12167 Grade CuAl11Fe6Ni6 H180Wrought Copper Bronze Aluminium Bronze
EN 12167 Grade CuAl11Fe6Ni6 H210Wrought Copper Bronze Aluminium Bronze
EN 12167 Grade CuAl11Fe6Ni6 R700Wrought Copper Bronze Aluminium Bronze
EN 12167 Grade CuAl11Fe6Ni6 R800Wrought Copper Bronze Aluminium Bronze
EN 12165 Grade CuAl11Fe6Ni6 MCast Copper Bronze Aluminium Bronze
CEN/TS 13388 Grade CB334G MCast Copper Bronze Aluminium Bronze
CEN/TS 13388 Grade CC334G M