Description

AMPCO-TRODE® 250 aluminum bronze bare filler rod is available for use with the gas tungsten arc welding process. The weld deposit has a nominal hardness of 250 Brinell and has higher yield strength and hardness than AMPCO-TRODE® 200 with lower tensile strength and ductility typical of the aluminum bronzes.


These characteristics make this deposit adaptable for use in extreme bearing applications where very high pressures are encountered.


AMPCO-TRODE® 250 is primarily used for overlay welding in applications where unusual wear-resistant qualities increase the service life of wearing parts.

Related Standards

Equivalent Materials

This material data has been provided by AMPCO METAL.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValue

Recycled Content

80 %

Show Supplier Material materials with Recycled Content of 80 %

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

0 %

Show Supplier Material materials with Elongation of 0 %

in 2″ (51 mm)

Hardness, Brinell

23.0 °C

340 [-]

Show Supplier Material materials with Hardness, Brinell of 340 [-]

BHN (3000kg) 1/4″ (6.4mm) deposit

Tensile strength

23.0 °C

538 MPa

Show Supplier Material materials with Tensile strength of 538 MPa

Yield strength

23.0 °C

386 MPa

Show Supplier Material materials with Yield strength of 386 MPa

Chemical properties

PropertyValueComment

Aluminium

13 - 14 %

Show Supplier Material materials with Aluminium of 13 - 14 %

Copper

Balance, including silver

Iron

3 - 5 %

Show Supplier Material materials with Iron of 3 - 5 %

Other

0.5 %

Show Supplier Material materials with Other of 0.5 %

max.

Silicon

0.04 %

Show Supplier Material materials with Silicon of 0.04 %

max.

Technological properties

Property
Application areas

Welding: Wear shoes, Chafing plates, Clutch fingers, Screw conveyors, Forming dies, Sleeves, Cams, Welding AMPCO® 22