Calcio: 3.5 %

Quick Comparison

Oxide Based Ceramic Matrix Composite

Fused Calcia-Stabilized Zirconia GNPPCK-a

Suministrada por:

GNPGraystar Specialty Materials

Oxide Based Ceramic Matrix Composite

Fused Calcia-Stabilized Zirconia GNPPCK-b

Suministrada por:

GNPGraystar Specialty Materials

Oxide Based Ceramic Matrix Composite

Fused Calcia-Stabilized Zirconia PCD

Suministrada por:

GNPGraystar Specialty Materials

Oxide Based Ceramic Matrix Composite

Fused Calcia-Stabilized Zirconia PCD-C

Suministrada por: