Fused Calcia-Stabilized Zirconia PCD-C

Want to keep this datasheet? Save it now in your required format

Description

GNPGraystar’s Fused Calcia-Stabilized Zirconia is produced by electro-fusion of high purity zirconia and calcia.

This material data has been provided by GNPGraystar Specialty Materials.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Density

5.8 g/cm³

Show Supplier Material materials with Density of 5.8 g/cm³

min.

Stabilization

75 %

Show Supplier Material materials with Stabilization of 75 %

85 %

Show Supplier Material materials with Stabilization of 85 %

Chemical properties

PropertyValueComment

Aluminium

0.1

Show Supplier Material materials with Aluminium of 0.1

Al₂O₃

Calcium

3.0 - 4.2 %

Show Supplier Material materials with Calcium of 3.0 - 4.2 %

CaO

Iron

0.1

Show Supplier Material materials with Iron of 0.1

max. Fe₂O₃

Silicon

0.2

Show Supplier Material materials with Silicon of 0.2

max. SiO₂

Titanium

0.1

Show Supplier Material materials with Titanium of 0.1

max. TiO₂

Zirconium

95 %

Show Supplier Material materials with Zirconium of 95 %

ZrO₂

Technological properties

Property
Application areas

GNPGraystar’s Fused Calcia-Stabilized Zirconia is used in various ceramic applications such as refractory setters for the electro-ceramic industry, zirconia furnace furniture, structural ceramics, sizing nozzles, zirconia hollow bead products, and more.

Color

Yellow

Other