Acero de alto carbono
EN 10270-1 Grade DH patented cold drawnAcero de alto carbono
EN 10270-1 Grade DM patented cold drawnAcero de alto carbono
EN 10270-1 Grade SH patented cold drawnAcero de alto carbono
JIS G3522 Grade SWP-BAcero de alto carbono
DIN 17223-1 Grade D patented cold drawnAcero de alto carbono
EN 10132-4 Grade C85S soft annealed or soft annealed and skin passed (+A or +A+LC)Acero de alto carbono
DIN 17222 Grade Ck85 cold rolled and hardenedAcero de alto carbono
EN 10270-1 Grade SL patented cold drawnAcero de alto carbono
EN 10270-1 Grade SM patented cold drawnAcero de alto carbono
DIN 17223-1 Grade B patented cold drawnAcero de alto carbono
DIN 17223-1 Grade 1.0500 patented cold drawnAcero para herramientas y maquinaria
EN 10132-4 Grade 80CrV2 soft annealed or soft annealed and skin passed (+A or +A+LC)Medium Carbon Steel
EN 10132-4 Grade C90S soft annealed or soft annealed and skin passed (+A or +A+LC)Acero de alto carbono
EN 10132-4 Grade C85S quenched and tempered (+QT)Acero inoxidable martensítico
EN 10090 Grade X85CrMoV18-2 quenched and tempered (+QT)Acero bajo en carbono
ISO 16120-2 Grade C82DAcero bajo en carbono
DIN 17140-1 Grade D 83-2Acero de alto carbono
EN 10132-4 Grade C85S cold rolled (+CR)Acero de alto carbono
EN 10132-4 Grade C85S quenched (+Q)Medium Carbon Steel
EN 10132-4 Grade C90S quenched and tempered (+QT)