JIS G3522 Grade SWP-B

Want to keep this datasheet? Save it now in your required format

Description

High tensile strength, high fatigue resistance

Related Standards

This material data has been provided by Japanese Industrial Standards,Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

7.8 g/cm³

Show Material materials with Density of 7.8 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

190 GPa

Show Material materials with Elastic modulus of 190 GPa

Elongation A50

23.0 °C

12 %

Show Material materials with Elongation A50 of 12 %

Hardness, Brinell

23.0 °C

190 [-]

Show Material materials with Hardness, Brinell of 190 [-]

Poisson's ratio

23.0 °C

0.29 [-]

Show Material materials with Poisson's ratio of 0.29 [-]

Typical for High Carbon Steel

Shear modulus

23.0 °C

81 GPa

Show Material materials with Shear modulus of 81 GPa

Typical for High Carbon Steel

Tensile strength

23.0 °C

1620 - 3480 MPa

Show Material materials with Tensile strength of 1620 - 3480 MPa

For Different Diameters

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.2E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.2E-5 1/K

Max service temperature

500 °C

Show Material materials with Max service temperature of 500 °C

Typical for Carbon Steel

Melting point

1410 °C

Show Material materials with Melting point of 1410 °C

Specific heat capacity

23.0 °C

470 J/(kg·K)

Show Material materials with Specific heat capacity of 470 J/(kg·K)

Thermal conductivity

23.0 °C

36 W/(m·K)

Show Material materials with Thermal conductivity of 36 W/(m·K)

Typical for High Carbon Steel

Electrical

PropertyTemperatureValueComment

Electrical resistivity

23.0 °C

1.43E-7 - 1.74E-7 Ω·m

Show Material materials with Electrical resistivity of 1.43E-7 - 1.74E-7 Ω·m

Typical for Carbon Steel

Chemical properties

PropertyValue

Carbon

0.6 - 0.95 %

Show Material materials with Carbon of 0.6 - 0.95 %

Copper

0.2 %

Show Material materials with Copper of 0.2 %

Manganese

0.3 - 0.9 %

Show Material materials with Manganese of 0.3 - 0.9 %

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Silicon

0.12 - 0.32 %

Show Material materials with Silicon of 0.12 - 0.32 %

Sulfur

0.025 %

Show Material materials with Sulfur of 0.025 %

Technological properties

Property
Application areas

Piano (Music) Wire

Corrosion properties

Not Corrosion Resistance