Carbon equivalent (CEV): 0.63 [-]

Quick Comparison

Acero para herramientas y maquinaria

DILLIDUR 400

Suministrada por:

Dillinger

Unclassified Low Alloy Steel

DILLIMAX 550 Basic (EN 1.8904)

Suministrada por:

Dillinger

Unclassified Low Alloy Steel

DILLIMAX 550 Tough (EN 1.8926)

Suministrada por:

Dillinger

Unclassified Low Alloy Steel

DILLIMAX 550 Extra Tough (EN 1.8986)

Suministrada por:

Dillinger

Unclassified Low Alloy Steel

DILLIMAX 500 Basic (EN 1.8924)

Suministrada por:

Dillinger

Unclassified Low Alloy Steel

DILLIMAX 500 Tough (EN 1.8924)

Suministrada por:

Dillinger

Unclassified Low Alloy Steel

DILLIMAX 500 Extra Tough (EN 1.8984)

Suministrada por:

Dillinger

Unclassified Low Alloy Steel

DILLIMAX 690 PE (EN 1.8879)

Suministrada por:

Dillinger

Acero para herramientas y maquinaria

DILLIDUR 600

Suministrada por:

Dillinger