Coefficient of friction, static: 0.36 [-]

Quick Comparison

Policarbonato (PC)

LNP™ LUBRILOY™ Compound DF2041

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ LUBRICOMP™ Compound DCP32 - Americas

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ LUBRICOMP™ Compound DCP32 - Asia

Suministrada por:

Sabic

Poliamida (PA)

LNP™ LUBRICOMP™ Compound VN001

Suministrada por:

Sabic

Polietersulfona (PES)

LNP™ LUBRICOMP™ Compound JFL36 - Americas

Suministrada por:

Sabic

Polietersulfona (PES)

LNP™ LUBRICOMP™ Compound JFL36 - Asia

Suministrada por:

Sabic

Polietersulfona (PES)

LNP™ LUBRICOMP™ Compound JFL36 - Europe