LNP™ LUBRICOMP™ Compound JFL36 - Asia

Want to keep this datasheet? Save it now in your required format

Description

LNP LUBRICOMP* JFL36 is a compound based on Polyethersulfone resin containing 30% Glass Fiber, 15% PTFE. Added featurs of this material is: Wear Resistant.

This material data has been provided by Sabic.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Coefficient of friction, kinetic

0.46 [-]

Show Supplier Material materials with Coefficient of friction, kinetic of 0.46 [-]

ASTM D 3702 Modified: Manual

Coefficient of friction, static

0.36 [-]

Show Supplier Material materials with Coefficient of friction, static of 0.36 [-]

ASTM D 3702 Modified: Manual

Density

23.0 °C

1.7 g/cm³

Show Supplier Material materials with Density of 1.7 g/cm³

ISO 1183

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

9.54 GPa

Show Supplier Material materials with Elastic modulus of 9.54 GPa

ISO 527 | 1 mm/min

Elongation

23.0 °C

1.6 %

Show Supplier Material materials with Elongation of 1.6 %

ISO 527 | break, 5 mm/min

Flexural modulus

23.0 °C

10.84 GPa

Show Supplier Material materials with Flexural modulus of 10.84 GPa

ISO 178

Flexural strength

23.0 °C

138 MPa

Show Supplier Material materials with Flexural strength of 138 MPa

ISO 178

Impact strength, Izod notched

23.0 °C

9 kJ/m²

Show Supplier Material materials with Impact strength, Izod notched of 9 kJ/m²

ISO 180/1A | 80*10*4, 23°C

Impact strength, Izod unnotched

23.0 °C

24 kJ/m²

Show Supplier Material materials with Impact strength, Izod unnotched of 24 kJ/m²

ISO 180/1U | unnotched 80*10*4, 23°C

Tensile strength

23.0 °C

117 MPa

Show Supplier Material materials with Tensile strength of 117 MPa

ISO 527 | break, 5 mm/min

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

2.28E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 2.28E-5 1/K

ISO 11359-2 | -40°C to 40°C

Coefficient of thermal expansion, transverse

23.0 °C

3.52E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion, transverse of 3.52E-5 1/K

ISO 11359-2 | -40°C to 40°C

Heat deflection temperature, 1.80 MPa

219 °C

Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 219 °C

ISO 75/Af | Flatw 80*10*4 sp=64mm

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

0.1 %

Show Supplier Material materials with Shrinkage of 0.1 %

ISO 294 | 24 hrs

Technological properties

Property
Application areas

Electronic Components

Availability

Europe,Asia,Americas

Features

Structural, Wear and Friction

Processing methods

Drying Temperature: 120 to 150.0°C
Front - Zone 3 Temperature: 370 to 380.0°C
Mold Temperature: 140 to 150.0°C
Rear - Zone 1 Temperature: 345 to 355.0°C
Screw Speed: 60 to 100.0rpm
Back Pressure: 0.3 to 0.7MPa
Melt Temperature: 355 to 370.0°C
Drying Time: 4hrs
Middle - Zone 2 Temperature: 360 to 370.0°C
Maximum Moisture Content: 0.05%

Supplier Disclaimer

While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right.