Coefficient of friction, static: 0.42 [-]

Quick Comparison

Polieterimida (PEI)

LNP™ LUBRICOMP™ Compound ECL36XXQ

Suministrada por:

Sabic

Tereftalato de polibutileno (PBT)

LNP™ LUBRICOMP™ Compound WFP36 - Americas

Suministrada por:

Sabic

Tereftalato de polibutileno (PBT)

LNP™ LUBRICOMP™ Compound WFP36 - Asia

Suministrada por:

Sabic

Tereftalato de polibutileno (PBT)

LNP™ LUBRICOMP™ Compound WFP36 - Europe

Suministrada por:

Sabic

Poliéter éter cetona (PEEK)

LNP™ LUBRICOMP™ Compound LX91475 - Europe

Suministrada por:

Sabic