Coefficient of friction: 0.34 [-]

Quick Comparison

Polyvinylidenefluoride (PVDF)

PVDF ISO-TECH

Suministrada por:

ISO-TECH Kunststoff GmbH

Policarbonato (PC)

LNP™ STAT-KON™ Compound DX05042

Suministrada por:

Sabic

Polioximetileno (POM)

LNP™ LUBRICOMP™ Compound KCL34A

Suministrada por:

Sabic

Polioximetileno (POM)

LNP™ STAT-LOY™ Compound K3000Z

Suministrada por:

Sabic

Polyphenylene Sulfide (PPS)

LNP™ LUBRICOMP™ Compound OCP36 - Asia

Suministrada por:

Sabic

Polyphenylene Sulfide (PPS)

LNP™ LUBRICOMP™ Compound OCP36 - Americas

Suministrada por:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRILOY™ Compound R2000

Suministrada por:

Sabic

Polyamide 610 (PA610)

LNP™ LUBRICOMP™ Compound QCL349

Suministrada por:

Sabic

Polyphenylene Sulfide (PPS)

LNP™ LUBRICOMP™ Compound OCP36A

Suministrada por:

Sabic

Polyamide 12 (PA12)

LNP™ LUBRICOMP™ Compound SCP36

Suministrada por:

Sabic

Polioximetileno (POM)

LNP™ STAT-KON™ Compound KEP33

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ LUBRICOMP™ Compound DL0039EF

Suministrada por:

Sabic

Polioximetileno (POM)

LNP™ STAT-LOY™ Compound K3000SZ

Suministrada por:

Sabic

Polioximetileno (POM)

LNP™ LUBRILOY™ Compound K2000

Suministrada por:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRICOMP™ Compound RCL34

Suministrada por:

Sabic

Polyamide 610 (PA610)

LNP™ LUBRICOMP™ Compound QCL34

Suministrada por:

Sabic

Polyamide 610 (PA610)

LNP™ LUBRICOMP™ Compound QL002

Suministrada por:

Sabic

Polioximetileno (POM)

LNP™ LUBRICOMP™ Compound KL001

Suministrada por:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRILOY™ Compound RF203

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ LUBRICOMP™ Compound DL003EXJ

Suministrada por:

Sabic
Página 1 de 4