PVDF ISO-TECH

Alternative and trade names
ISO-PVDF
Want to keep this datasheet? Save it now in your required format

Description

ISO-PVDF is a thermoplastic with good mechanical properties. Thanks to its high resistance to chemicals, our customers particularly in the chemical and pharmaceutical industries use this material, especially in systems with high mechanical stress. The key features are:


  • High chemical resistance
  • High abrasion resistance
  • Very low moisture absorption
  • Related Standards

    This material data has been provided by ISO-TECH Kunststoff GmbH.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyValueComment

    Coefficient of friction

    0.34 [-]

    Show Supplier Material materials with Coefficient of friction of 0.34 [-]

    DIN 53375, C, Against dry running steel

    Density

    1.78 g/cm³

    Show Supplier Material materials with Density of 1.78 g/cm³

    ISO 1183

    Water absorption

    0.04 %

    Show Supplier Material materials with Water absorption of 0.04 %

    max., ISO 62

    Mechanical

    PropertyValueComment

    Elastic modulus

    2 GPa

    Show Supplier Material materials with Elastic modulus of 2 GPa

    ISO 527

    Elongation

    50 %

    Show Supplier Material materials with Elongation of 50 %

    min., ISO 527

    Elongation at yield

    9 %

    Show Supplier Material materials with Elongation at yield of 9 %

    ISO 527

    Flexural strength

    80 MPa

    Show Supplier Material materials with Flexural strength of 80 MPa

    ISO 178

    Hardness, Ball Indentation

    80 MPa

    Show Supplier Material materials with Hardness, Ball Indentation of 80 MPa

    ISO 2039-1

    Hardness, Shore D

    78 [-]

    Show Supplier Material materials with Hardness, Shore D of 78 [-]

    DIN 53505

    Impact strength, Charpy notched

    22 kJ/m²

    Show Supplier Material materials with Impact strength, Charpy notched of 22 kJ/m²

    ISO 179

    Impact strength, Charpy unnotched

    252 kJ/m²

    Show Supplier Material materials with Impact strength, Charpy unnotched of 252 kJ/m²

    ISO 179

    Yield strength

    50 MPa

    Show Supplier Material materials with Yield strength of 50 MPa

    ISO 527

    Thermal

    PropertyValuePressureComment

    Coefficient of thermal expansion

    0.00015 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 0.00015 1/K

    DIN 53752

    Heat deflection temperature

    104 °C

    Show Supplier Material materials with Heat deflection temperature of 104 °C

    2 MPa

    145 °C

    Show Supplier Material materials with Heat deflection temperature of 145 °C

    0.45 MPa

    Max service temperature

    150 °C

    Show Supplier Material materials with Max service temperature of 150 °C

    Longterm

    Long

    Short

    Min service temperature

    -30 °C

    Show Supplier Material materials with Min service temperature of -30 °C

    Longterm

    Thermal conductivity

    0.13 W/(m·K)

    Show Supplier Material materials with Thermal conductivity of 0.13 W/(m·K)

    DIN 52612

    Vicat softening temperature

    138 °C

    Show Supplier Material materials with Vicat softening temperature of 138 °C

    ISO 306, VST B50

    Flammability

    V-0 UL 94

    Electrical

    PropertyValueComment

    Comparative tracking index

    600 V

    Show Supplier Material materials with Comparative tracking index of 600 V

    IEC 60112

    Dielectric constant

    7 [-]

    Show Supplier Material materials with Dielectric constant of 7 [-]

    DIN 53483

    Dielectric strength

    27 kV/mm

    Show Supplier Material materials with Dielectric strength of 27 kV/mm

    VDE 0303

    Loss tangent

    0.24 [-]

    Show Supplier Material materials with Loss tangent of 0.24 [-]

    DIN 53483

    Surface resistivity

    1e+10 Ω/sq

    Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq

    min., VDE 0303

    Volume resistivity

    1e+10 Ω·cm

    Show Supplier Material materials with Volume resistivity of 1e+10 Ω·cm

    min., VDE 0303

    Technological properties

    Property
    Application areas