Wrought Copper Nickel Silver Grade
EN 12164 Grade CuNi12Zn30Pb1 R420Other Copper Zinc Alloy
EN 12164 Grade CuZn37Mn3Al2PbSi R590Other Copper Zinc Alloy
EN 12164 Grade CuZn37Mn3Al2PbSi R540Other Copper Zinc Alloy
EN 12164 Grade CuZn37Mn3Al2PbSi R640Other Copper Zinc Alloy
EN 12168 Grade CuZn37Mn3Al2PbSi H130Other Copper Zinc Alloy
EN 12168 Grade CuZn37Mn3Al2PbSi H150Other Copper Zinc Alloy
EN 12164 Grade CuZn37Mn3Al2PbSi H170Other Copper Zinc Alloy
EN 12164 Grade CuZn37Mn3Al2PbSi R570Other Copper Zinc Alloy
EN 12164 Grade CuZn37Mn3Al2PbSi R620Wrought Copper Nickel Silver Grade
EN 12164 Grade CuNi12Zn30Pb1 R650Wrought Copper Nickel Silver Grade
EN 12167 Grade CuNi12Zn30Pb1 R430Wrought Copper Nickel Silver Grade
EN 12167 Grade CuNi12Zn30Pb1 R480Other Copper Zinc Alloy
EN 12167 Grade CuZn37Mn3Al2PbSi H160Leaded Brass
EN 12167 Grade CuZn43Pb2 H110Leaded Brass
EN 12167 Grade CuZn43Pb2 H130Leaded Brass
EN 12167 Grade CuZn43Pb2 R430Leaded Brass
EN 12167 Grade CuZn43Pb2 R480