Wrought Copper Nickel Silver Grade
ASTM B122 Grade C73500 H06Wrought Copper Nickel Silver Grade
ASTM B122 Grade C73500 H01Wrought Copper Nickel Silver Grade
ASTM B122 Grade C73500 H02Wrought Copper Nickel Silver Grade
ASTM B122 Grade C73500 H04Wrought Copper Bronze Aluminium Bronze
EN 12167 Grade CuAl11Fe6Ni6 H180Cast Copper Brass Yellow Brass
ASTM B584 Grade C85200Wrought Copper Nickel Silver Grade
ASTM B122 Grade C73500 OS015Cast Copper Brass Yellow Brass
ASTM B271 Grade C85200 As-CastWrought Copper Nickel Silver Grade
ASTM B122 Grade C73500 OS035Cast Copper Brass Yellow Brass
ASTM B584 Grade C85200Cast Copper Brass Yellow Brass
ASTM B763 Grade C85200 Separately Cast Test BarsWrought Copper Nickel Silver Grade
ASTM B122 Grade C74000 H01Wrought Copper Nickel Silver Grade
ASTM B122 Grade C74000 H04Wrought Copper Nickel Silver Grade
ASTM B122 Grade C74000 H02Wrought Copper Nickel Silver Grade
ASTM B122 Grade C74000 H06Wrought Copper Nickel Grade
UNS C71000 O61Wrought Copper Nickel Silver Grade
ASTM B122 Grade C74000 M20Wrought Copper Nickel Silver Grade
ASTM B122 Grade C74000 OS035Wrought Copper Nickel Silver Grade
ASTM B122 Grade C74000 OS070