CEN/TS 13388 Grade CW703R R660, H190

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.2 g/cm³

Show Material materials with Density of 8.2 g/cm³

Dimension

PropertyValue

Dimensions

Dicke

Mechanical

PropertyTemperatureValue

Bending angle 90°

20.0 °C

0 - 1 °/t

Show Material materials with Bending angle 90° of 0 - 1 °/t

Elastic modulus

20.0 °C

115 GPa

Show Material materials with Elastic modulus of 115 GPa

Elongation A50

20.0 °C

8 - 10 %

Show Material materials with Elongation A50 of 8 - 10 %

Hardness, Vickers

20.0 °C

190 - 220 [-]

Show Material materials with Hardness, Vickers of 190 - 220 [-]

Tensile strength

20.0 °C

660 - 750 MPa

Show Material materials with Tensile strength of 660 - 750 MPa

Yield strength Rp0.2

20.0 °C

580 MPa

Show Material materials with Yield strength Rp0.2 of 580 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

20.0 °C

1.82E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.82E-5 1/K

100.0 °C

1.82E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.82E-5 1/K

Thermal conductivity

20.0 °C

78 W/(m·K)

Show Material materials with Thermal conductivity of 78 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

20.0 °C

1.00E+7 S/m

Show Material materials with Electrical conductivity of 1.00E+7 S/m

Electrical resistivity

20.0 °C

1E-7 Ω·m

Show Material materials with Electrical resistivity of 1E-7 Ω·m

Chemical properties

PropertyValue

Aluminium

3 - 3.8 %

Show Material materials with Aluminium of 3 - 3.8 %

Cobalt

0.25 - 0.55 %

Show Material materials with Cobalt of 0.25 - 0.55 %

Copper

72 - 75 %

Show Material materials with Copper of 72 - 75 %

Iron

0.05 %

Show Material materials with Iron of 0.05 %

Lead

0.05 %

Show Material materials with Lead of 0.05 %

Nickel

0.3 %

Show Material materials with Nickel of 0.3 %

Other

Rest Zn, total 0.1

Tin

0.1 %

Show Material materials with Tin of 0.1 %