Creep strength 10^4 cycles: 10 MPa

Quick Comparison

Acero inoxidable ferrítico

Sandvik 4C54

Suministrada por:

Alleima (formerly Sandvik Materials Technology)

Acero inoxidable austenítico

Sandvik 7RE10

Suministrada por:

Alleima (formerly Sandvik Materials Technology)