Factor de disipación: 270 [-]

Quick Comparison

Polyamide 6 (PA6)

Akulon® K224-HG3

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® K224-HG0

Suministrada por:

DSM Engineering Materials

Polyamide 6 (PA6)

Akulon® Ultraflow K-FHG0

Suministrada por:

DSM Engineering Materials

Poliftalamida (PPA)

ForTii® MX3

Suministrada por:

DSM Engineering Materials

Polyamide 4T (PA4T)

ForTii® MX2

Suministrada por:

DSM Engineering Materials