Módulo elástico: 19.6 GPa

Quick Comparison

Policarbonato (PC)

LNP™ STAT-KON™ Compound DE006

Suministrada por:

Sabic

Polímero

Liquid-crystalline polymer (LCP)

Suministrada por:

1 proveedor Matmatch

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RF00C - Americas

Suministrada por:

Sabic

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RF00C - Europe

Suministrada por:

Sabic