Moso Bamboo

Want to keep this datasheet? Save it now in your required format

Description

Moso bamboo is one of the commercially most important bamboo species. Being ready for harvest in less than ten years, bamboo products are ideal for sustainable construction and resource-efficient product design.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

0.5 - 0.65 g/cm³

Show Material materials with Density of 0.5 - 0.65 g/cm³

Mechanical

PropertyTemperatureValue

Compressive strength

20.0 °C

40 - 110 MPa

Show Material materials with Compressive strength of 40 - 110 MPa

Elastic modulus

20.0 °C

5 - 20 GPa

Show Material materials with Elastic modulus of 5 - 20 GPa

Hardness, Brinell

20.0 °C

45 - 63 [-]

Show Material materials with Hardness, Brinell of 45 - 63 [-]

Tensile strength

20.0 °C

100 - 400 MPa

Show Material materials with Tensile strength of 100 - 400 MPa

Thermal

PropertyTemperatureValue

Specific heat capacity

20.0 °C

1400 - 1800 J/(kg·K)

Show Material materials with Specific heat capacity of 1400 - 1800 J/(kg·K)

Thermal conductivity

20.0 °C

0.16 - 0.22 W/(m·K)

Show Material materials with Thermal conductivity of 0.16 - 0.22 W/(m·K)

Thermal diffusivity

20.0 °C

0.24 - 0.62 mm²/s

Show Material materials with Thermal diffusivity of 0.24 - 0.62 mm²/s