Temperatura de transición del vidrio: 85 °C

Quick Comparison

Other Polyamide (PA)

Zytel® HTN53G50HSLR BK083

Polyamide 66 (PA66)

Zytel® PLS95G35DH1 BK549

Other Polyamide (PA)

Zytel® HTN53G50HSLR NC010

Fraguado térmico

OptiStack® SOC110E

Suministrada por: