Description

spin-on thermoset material solution, with a high carbon content, planarization properties

This material data has been provided by Brewer Science.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Thermal

PropertyValueComment

Glass transition temperature

42158 °C

Show Supplier Material materials with Glass transition temperature of 42158 °C

respectively for before and after cross linking (205°C/60s bake)

Max service temperature

290 °C

Show Supplier Material materials with Max service temperature of 290 °C

Technological properties

Property
Application areas

Surface Planarization, High Temperature Gap fill, Spin-on Carbon, High temperature thermoset, Semiconductor Industry, Aerospace, Automotive, Packaging, Electronic Packaging