Dureza Brinell (HBW): 244.4 [-]

Quick Comparison

Cast Copper Brass Yellow Brass

ASTM B505 Grade C86500

Suministrada por:

1 proveedor Matmatch

Cast Copper Brass Yellow Brass

ASTM B584 Grade C86400

Suministrada por:

1 proveedor Matmatch

Hierro fundido

SAE J434 Grade D5506

Hierro fundido

SAE J434 Grade D7003