Dureza Brinell (HBW): 183 [-]

Quick Comparison

Wrought Copper Bronze Aluminium Bronze

AMPCO® 8 Extruded and drawn rods

Suministrada por:

AMPCO METAL

Cast Copper Bronze Aluminium Bronze

AMPCO® 18 Centrifugal castings

Suministrada por:

AMPCO METAL

Cast Copper Bronze Aluminium Bronze

AMPCO® 18 Continuous cast

Suministrada por:

AMPCO METAL

Medium Carbon Steel

SAE J435 Grade 0030

Hierro fundido

SAE J434 Grade D4512