Dureza Vickers 10: 235 [-]

Quick Comparison

Molibdeno

Molybdenum Ground Rod

Suministrada por:

Plansee

Molibdeno

Molybdenum Smooth Forged Rod

Suministrada por:

Plansee

Molibdeno

Molybdenum Coarse Forged Rod

Suministrada por:

Plansee

Molibdeno

Molybdenum Extruded Rod

Suministrada por:

Plansee