Heat deflection temperature, 0.45 MPa: 257 °C

Quick Comparison

Polyamide 66 (PA66)

Zytel® BM70G20HSLX BK537

Polyamide 66 (PA66)

LNP™ LUBRICOMP™ Compound RFN169

Suministrada por:

Sabic

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RF006XXY

Suministrada por:

Sabic

Polyamide 66 (PA66)

LNP™ STAT-KON™ Compound RFD04

Suministrada por:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRICOMP™ Compound RFL32

Suministrada por:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRICOMP™ Compound RFP38

Suministrada por:

Sabic