General
Property | Temperature | Value | Comment |
---|---|---|---|
Density | 23.0 °C | 1.4 g/cm³ Show Supplier Material materials with Density of 1.4 g/cm³ | ASTM D 792 |
Moisture absorption | 23.0 °C | 0.89 % Show Supplier Material materials with Moisture absorption of 0.89 % | ISO 62 | (23°C / 50% RH) |
Relative density | 23.0 °C | 1.4 [-] Show Supplier Material materials with Relative density of 1.4 [-] | ASTM D 792 | |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 11.6 GPa Show Supplier Material materials with Elastic modulus of 11.6 GPa | ISO 527 | 1 mm/min |
Elongation | 23.0 °C | 2.7 % Show Supplier Material materials with Elongation of 2.7 % | ISO 527 | yield, 5 mm/min |
Flexural modulus | 23.0 °C | 10 GPa Show Supplier Material materials with Flexural modulus of 10 GPa | ISO 178 | 2 mm/min |
Flexural strength | 23.0 °C | 275 MPa Show Supplier Material materials with Flexural strength of 275 MPa | ISO 178 |
Impact strength, Izod notched | 23.0 °C | 10 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 10 kJ/m² | ISO 180/1A | 80*10*4, 23°C |
Impact strength, Izod notched, ASTM | 23.0 °C | 107 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 107 J/m | ASTM D 256 |
Impact strength, Izod unnotched | 23.0 °C | 61 kJ/m² Show Supplier Material materials with Impact strength, Izod unnotched of 61 kJ/m² | ISO 180/1U | unnotched 80*10*4 |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 1100 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 1100 J/m | ASTM D 4812 | 23°C |
Instrumented Impact, Total Energy | 23.0 °C | 9 J Show Supplier Material materials with Instrumented Impact, Total Energy of 9 J | ASTM D 3763 | 23°C |
Tensile strength | 23.0 °C | 183 MPa Show Supplier Material materials with Tensile strength of 183 MPa | ISO 527 | break, 5 mm/min |
Thermal
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 2.5E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 2.5E-5 1/K | ASTM D 696 | -30°C to 30°C | ||
Coefficient of thermal expansion, transverse | 23.0 °C | 6.7E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion, transverse of 6.7E-5 1/K | ASTM D 696 | -30°C to 30°C | ||
Heat deflection temperature | 246 - 257 °C Show Supplier Material materials with Heat deflection temperature of 246 - 257 °C | ||||
Heat deflection temperature, 0.45 MPa | 257 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 257 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 246 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 246 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | UL 746B | |||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | UL 746B | |||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | UL 746B | |||
Flammability | UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=101282588- - <br> UL Recognized, 94HB Flame Class Rating: 1.5mm UL 94 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Medical Device | |
Availability | Europe,Asia,Americas | |
Processing methods | Drying Temperature: 80°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |