Policarbonato (PC)
LEXAN™ Healthcare Resin HP2NRPolicarbonato (PC)
LEXAN™ Healthcare Resin HP2Policarbonato (PC)
LEXAN™ Healthcare Resin HP4Policarbonato (PC)
LEXAN™ Healthcare Resin HP2REUPolicarbonato (PC)
LEXAN™ Healthcare Resin HP4RPolicarbonato (PC)
LEXAN™ Healthcare Resin HP4REUPolicarbonato (PC)
LEXAN™ Healthcare Resin HPS2