Resistencia al choque, ensayo Charpy no entallado: 208 kJ/m²

Quick Comparison

Polyvinylidenefluoride (PVDF)

Kynar® 720

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar® 720 RED

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar® 720 MED

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar® 710

Suministrada por:

Arkema: High Performance Polymers