Impact strength, Izod notched, ASTM: 780 J/m

Quick Comparison

Policarbonato (PC)

LEXAN™ Copolymer SLX2271T - Asia

Suministrada por:

Sabic

Policarbonato (PC)

LEXAN™ Copolymer SLX2271T - Americas

Suministrada por:

Sabic

Policarbonato (PC)

LEXAN™ Copolymer SLX9271T - Europe

Suministrada por:

Sabic