Description

Poly(butene-1) exhibits excellent creep properties. It is tough, retains strength at elevated temperatures, and is resistant to stress cracking and abrasion.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.86 g/cm³

Show Material materials with Density of 0.86 g/cm³

Water absorption

23.0 °C

0.03 %

Show Material materials with Water absorption of 0.03 %

ma., ASTM D570, 24h

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

0.29 - 0.3 GPa

Show Material materials with Elastic modulus of 0.29 - 0.3 GPa

ASTM D638

Elongation

23.0 °C

275 - 320 %

Show Material materials with Elongation of 275 - 320 %

ASTM D638

Flexural modulus

23.0 °C

0.38 GPa

Show Material materials with Flexural modulus of 0.38 GPa

ASTM D790

Hardness, Shore D

23.0 °C

55 - 65 [-]

Show Material materials with Hardness, Shore D of 55 - 65 [-]

ASTM D2240

Impact strength, Izod notched, ASTM

23.0 °C

640 - 800 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 640 - 800 J/m

ASTM D256

Poisson's ratio

25.0 °C

0.47 [-]

Show Material materials with Poisson's ratio of 0.47 [-]

Tensile strength

23.0 °C

32 - 35 MPa

Show Material materials with Tensile strength of 32 - 35 MPa

ASTM D638

Yield strength

23.0 °C

16 - 18 MPa

Show Material materials with Yield strength of 16 - 18 MPa

ASTM D638

Thermal

PropertyTemperatureValueComment

Brittleness temperature

-18.15 °C

Show Material materials with Brittleness temperature of -18.15 °C

ASTM D746

Coefficient of thermal expansion

23.0 °C

6.7E-4 1/K

Show Material materials with Coefficient of thermal expansion of 6.7E-4 1/K

for 140 to 240°C

Glass transition temperature

248 - 256 °C

Show Material materials with Glass transition temperature of 248 - 256 °C

DMA

Heat deflection temperature, 0.45 MPa

101.85 - 112.85 °C

Show Material materials with Heat deflection temperature, 0.45 MPa of 101.85 - 112.85 °C

ASTM D648

Heat deflection temperature, 1.80 MPa

53.85 - 59.85 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 53.85 - 59.85 °C

ASTM D648

Thermal conductivity

23.0 °C

0.22 W/(m·K)

Show Material materials with Thermal conductivity of 0.22 W/(m·K)

ASTM C177

Electrical

PropertyTemperatureValue

Dielectric constant, 100Hz

23.0 °C

2.53 [-]

Show Material materials with Dielectric constant, 100Hz of 2.53 [-]

Dissipation factor, 100Hz

23.0 °C

5E-4 [-]

Show Material materials with Dissipation factor, 100Hz of 5E-4 [-]

Optical

PropertyValue

Refractive index

1.51 [-]

Show Material materials with Refractive index of 1.51 [-]

Rheological Properties

PropertyValueComment

Melt mass-flow rate

0.4 g/10min

Show Material materials with Melt mass-flow rate of 0.4 g/10min

ASTM D 1238(E)

Technological properties

Property
Application areas

Hot water and high-pressure piping, films, adhesives, comonomer for ethylene polymers. Atactic polymer is used in sealants.