Impact strength, Izod notched, ASTM: 23 J/m

Quick Comparison

Policarbonato (PC)

LNP™ STAT-KON™ Compound DD0001

Suministrada por:

Sabic

Acrilonitrilo estireno acrilato

GELOY™ Resin FXTW26SK

Éter de polifenileno (PPE)

NORYL™ Resin ZM3242C - Asia

Suministrada por:

Sabic

Éter de polifenileno (PPE)

NORYL™ Resin ZM3242 - Asia

Suministrada por:

Sabic

Estireno acrilonitrilo (SAN)

CYCOLAC™ Resin INP562

Estireno acrilonitrilo (SAN)

CYCOLAC™ Resin INP581