Low flow powder SAN for color concentrates and alloys. FDA compliant (part use must be at room temperature or below).

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.08 g/cm³

Show Material materials with Density of 1.08 g/cm³

ASTM D 792

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

3.83 GPa

Show Material materials with Elastic modulus of 3.83 GPa

ASTM D 638 | 5 mm/min

Elongation

23.0 °C

2.9 %

Show Material materials with Elongation of 2.9 %

ASTM D 638 | Type I, 5 mm/min

Elongation at yield

23.0 °C

2.9 %

Show Material materials with Elongation at yield of 2.9 %

ASTM D 638 | Type I, 5 mm/min

Flexural modulus

23.0 °C

3.46 GPa

Show Material materials with Flexural modulus of 3.46 GPa

ISO 178 | 2 mm/min

Flexural yield strength

23.0 °C

74 MPa

Show Material materials with Flexural yield strength of 74 MPa

ISO 178 | 2 mm/min

Hardness, Rockwell R

23.0 °C

121 [-]

Show Material materials with Hardness, Rockwell R of 121 [-]

ASTM D 785

Impact strength, Charpy notched

23.0 °C

1 kJ/m²

Show Material materials with Impact strength, Charpy notched of 1 kJ/m²

ISO 179/2C

Impact strength, Izod notched

-30.0 °C

2 kJ/m²

Show Material materials with Impact strength, Izod notched of 2 kJ/m²

ISO 180/1A

23.0 °C

2 kJ/m²

Show Material materials with Impact strength, Izod notched of 2 kJ/m²

ISO 180/1A

Impact strength, Izod notched, ASTM

-30.0 °C

23 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 23 J/m

ASTM D 256

23.0 °C

22 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 22 J/m

ASTM D 256

Unlock all property charts

Tensile strength

23.0 °C

74 MPa

Show Material materials with Tensile strength of 74 MPa

ASTM D 638 | Type I, 5 mm/min

Yield strength

23.0 °C

74 MPa

Show Material materials with Yield strength of 74 MPa

ASTM D 638 | Type I, 5 mm/min

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

84 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 84 °C

ASTM D 648 | 1.82 MPa, 3.2mm, unannealed

Vicat softening temperature

106 °C

Show Material materials with Vicat softening temperature of 106 °C

ISO 306 | Rate B/120

Rheological Properties

PropertyValueComment

Melt mass-flow rate

16 g/10min

Show Material materials with Melt mass-flow rate of 16 g/10min

ISO 1133 | 220°C/10.0 kg