Instrumented Impact, at Peak: 12 J

Quick Comparison

Polyamide 66 (PA66)

LNP™ LUBRILOY™ Compound RF206

Suministrada por:

Sabic

Polyamide 66 (PA66)

LNP™ THERMOCOMP™ Compound RF00AS

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ STAT-KON™ Compound DEL339XF

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ STAT-KON™ Compound DD0009P

Suministrada por:

Sabic

Polyamide 66 (PA66)

LNP™ LUBRICOMP™ Compound RFL36L

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ STAT-KON™ Compound DD0009PC - Europe

Suministrada por:

Sabic

Polyamide 6 (PA6)

LNP™ THERMOCOMP™ Compound PF008QS

Suministrada por:

Sabic

Polietersulfona (PES)

LNP™ THERMOCOMP™ Compound JF006LZZ

Suministrada por:

Sabic

Policarbonato (PC)

LNP™ THERMOCOMP™ Compound DC006

Suministrada por:

Sabic