Índice límite de óxigeno: 75 %

Quick Comparison

Polyvinylidenefluoride (PVDF)

Kynar Flex® 2900-04

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Superflex® 2500-25

Suministrada por:

Arkema: High Performance Polymers

Polyvinylidenefluoride (PVDF)

Kynar Flex® 3030-15

Suministrada por:

Arkema: High Performance Polymers