Kynar Flex® 3030-15

Alternative and trade names
PVDF
Want to keep this datasheet? Save it now in your required format

Description

Kynar Flex® 3030-15 resin is a copolymer of vinylidene fluoride and hexafluoropropylene specifically designed for flexible plenum cables and tubing.

Its main characteristics are:

  • Very high flexibility
  • High melting point
  • Excellent low temperature impact resistance
  • Plenum rated

  • This material data has been provided by Arkema High Performance Polymers.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    General

    PropertyTemperatureValueComment

    Limiting oxygen index

    23.0 °C

    90 %

    Show Supplier Material materials with Limiting oxygen index of 90 %

    ISO 4589-1/-2

    Mechanical

    PropertyTemperatureValueComment

    Elastic modulus

    23.0 °C

    0.29 GPa

    Show Supplier Material materials with Elastic modulus of 0.29 GPa

    ISO 527-1/-2

    Elongation

    23.0 °C

    50 %

    Show Supplier Material materials with Elongation of 50 %

    min., ISO 527-1/-2, nominal

    Elongation at yield

    23.0 °C

    30 %

    Show Supplier Material materials with Elongation at yield of 30 %

    ISO 527-1/-2

    Yield strength

    23.0 °C

    12 MPa

    Show Supplier Material materials with Yield strength of 12 MPa

    ISO 527-1/-2

    Impact strength, Charpy notched

    No break @ 23°C, ISO 179/1eA

    Thermal

    PropertyValueComment

    Glass transition temperature

    -40 °C

    Show Supplier Material materials with Glass transition temperature of -40 °C

    ISO 11357-1/-2, 10°C/min

    Melting point

    164 °C

    Show Supplier Material materials with Melting point of 164 °C

    ISO 11357-1/-3, 10°C/min

    Flammability

    At thickness 0.8 mm IEC 60695-11-10: V-0

    Electrical

    PropertyTemperatureValueComment

    Volume resistivity

    23.0 °C

    2.00E+14 Ω·cm

    Show Supplier Material materials with Volume resistivity of 2.00E+14 Ω·cm

    IEC 60093

    Technological properties

    Property
    Application areas

    Auto - Water Cooling Circuit,Automotive Cables,Foamed PVDF Cable Jacketing,Performance Wire,Plenum Cable,Plenum Conduit,PVDF Cable Jacketing,Wire and Cables