Chromium Molybdenum Steel
EN 10028-2 Grade 13CrMo4-5 normalized and tempered (+NT)Suministrada por:
1 proveedor Matmatch
Chromium Molybdenum Steel
EN 10028-2 Grade 13CrMo4-5 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Acero inoxidable ferrítico
DIN 17440 Grade X6Cr17 soft annealed (+A)Acero inoxidable austenítico
DIN 17440 Grade X5CrNi18-10 quenched (+Q)Acero inoxidable austenítico
DIN 17440 Grade X5CrNi18-10 solution heat-treated and quenchedAcero inoxidable austenítico
DIN 17440 Grade X6CrNiNb18-10 solution heat-treated and quenchedAcero inoxidable austenítico
DIN 17440 Grade X5CrNiMo17-12-2 solution heat-treated and quenchedAcero inoxidable austenítico
DIN 17440 Grade X5CrNiMo17-12-2 quenched (+Q)Acero inoxidable austenítico
DIN 17440 Grade X6CrNiNb18-10 quenched (+Q)Acero inoxidable austenítico
EN 10028-7 Grade X5CrNi18-10 solution annealed (+AT)