Acero inoxidable ferrítico
DIN 17440 Grade X6Cr17 soft annealed (+A)Acero inoxidable martensítico
EN 10088-1 Grade X6Cr13 soft annealed (+A)Acero inoxidable martensítico
DIN 17440 Grade X6Cr13 soft annealed (+A)Acero inoxidable austenítico
EN 10095 Grade X15CrNiSi20-12 solution annealed (+AT)Acero inoxidable austenítico
SEW 470 Grade X15CrNiSi20-12 solution annealed (+AT)Acero inoxidable austenítico
EN 10270-3 Grade X5CrNiMo17-12-2 cold drawnAcero inoxidable ferrítico
EN 10095 Grade X18CrN28 soft annealed (+A)Acero inoxidable ferrítico
DIN 1654-5 Grade X6Cr17 soft annealed (+A)Acero inoxidable ferrítico
DIN 1654-5 Grade X6Cr17 annealed to achieve spheroidized carbides (+AC)Acero inoxidable ferrítico
DIN 1654-5 Grade X6Cr17 annealed to achieve spheroidized carbides and turnedAcero inoxidable ferrítico
DIN 1654-5 Grade X6Cr17 cold drawn, annealed to achieve spheroidized carbides and slightly skin passedAcero inoxidable ferrítico
EN 10250-4 Grade X6Cr17 soft annealed (+A)Acero inoxidable ferrítico
DIN 17440 Grade X6Cr17 heat treated