Resistencia al cizallamiento: 600.6 MPa

Quick Comparison

Unclassified Low Alloy Steel

EN 10025-6 Grade S690QL1 quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch

Unclassified Low Alloy Steel

EN 10025-6 Grade S690QL quenched and tempered (+QT)

Suministrada por:

1 proveedor Matmatch