Specific heat capacity melt: 1930 J/(kg·K)

Quick Comparison

Polyamide 46 (PA46)

Stanyl® TW200F8

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TW241F8

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TE200F8

Suministrada por:

DSM Engineering Materials

Polyamide 46 (PA46)

Stanyl® TS200F8

Suministrada por:

DSM Engineering Materials