Leaded Phosphor Bronze
DIN 1733-1 Grade 2.1027Cast Copper Brass Yellow Brass
ISO 1338 Grade CuZn33Pb2Leaded Tin Bronze
ASTM B505 Grade C92500Leaded Tin Bronze
ASTM B505 Grade C92500Leaded Tin Bronze
ASTM B505 Grade C94000Tin Bronze
ASTM B505 Grade C91000Tin Bronze
ASTM B505 Grade C91000Leaded Tin Bronze
ASTM B505 Grade C94000Tin Bronze
CEN/TS 13388 Grade 423123Leaded Brass
CEN/TS 13388 Grade C-3120Tin Bronze
DS 3001 Grade 5465Leaded Tin Bronze
DS 3001 Grade 5475Tin Bronze
SIS 145465 Grade 5465Leaded Tin Bronze
SIS 145475 Grade 5475Tin Bronze
AS/NZS 1565 Grade C90250Tin Bronze
ASTM B30 Grade C90800Tin Bronze
AS/NZS 1565 Grade C90810Tin Bronze
AS/NZS 1565 Grade C91700